Gas Sheilded Flux-Cored Wire for Stainless Steel

Delivery term:The date of payment from buyers deliver within days
  • Price:

    Negotiable

  • minimum:

  • Total supply:

  • Delivery term:

    The date of payment from buyers deliver within days

  • seat:

    Shandong

  • Validity to:

    Long-term effective

  • Last update:

    2017-12-04 08:45

  • Browse the number:

    889

Send an inquiries
+
Qingdao Kingdom Cheer Industry Co.,Ltd
Contactaixin:

Contactaixin:

qdqwf(Mr.)  

Email:

telephone:

phone:

Area:

Shandong

Address:

No. 32, Hongkong Middle Road, Shinan District., Qingdao, Shandong, China

Website:

http://www.cnkingdomcheer.com/ http://www.ey0558.com/com/qdqwf/

+





















































































































































































Gas Shielded F.C.W for Stainless Steel




 




Product Name




Equivalent Standard




Chemical Composition of Deposited Metal(%)




Mechanical Properties of Deposited Metal




Characteristics and Applications




AWS




JIS




C




Mn




Si




S




P




Ni




Cr




Mo




σs(MPa)




σb(MPa)




δ5%




Akv(J) Room temperature




KDC-YA308(Q)




E308T-1




YF308C




0.050




1.45




0.52




0.008




0.018




9.8




19.2




/




/




570




40




37(0℃)




For welding18%Cr-8%Ni stainless steels.




KDC-YA308L(Q)




E308LT-1




YF308LC




0.030




1.42




0.5




0.008




0.015




10.5




19.5




/




/




550




43




42(0℃)




For welding 18%Cr-8%Ni extra- low carbon stainless steel.




KDC-YA309(Q)




E309T-1




YF309C




0.045




1.25




0.48




0.009




0.012




12.4




24.2




0.03




/




595




32




32(0℃)




For welding dissimilar steel and Cladding Steel Shee,and using in the transition layer welding when surfacing stainless steel.




KDC-YA309L(Q)




E309LT-1




YF309LC




0.025




1.32




0.53




0.010




0.017




13.2




24.5




0.05




/




590




30




/




KDC-YA309Mo(Q)




/




YF309MoC




0.050




1.24




0.49




0.009




0.015




13.2




23.2




2.75




/




690




30




/




KDC-YA316(Q)




E316T-1




YF316C




0.040




1.50




0.51




0.010




0.019




12.8




19.5




2.41




/




570




40




40(0℃)




For welding 18%Cr-8%Ni stainless steels.




KDC-YA316L(Q)




E316LT-1




YF316LC




0.028




1.45




0.52




0.010




0.017




12.4




18.7




2.52




/




540




40




42(0℃)




For welding 18%Cr-12%Mo extra-low carbon stainless steel.




KDC-YA347(Q)




E347T-1




YF347C




0.040




1.21




0.42




0.008




0.015




10.3




18.7




/




/




600




41




50(0℃)




For welding 18%Cr-8%Ni -Nb or 18%Cr-8%Ni stainless steels.




KDC-YA410(Q)




E410T-1




YF410C




0.050




1.00




0.47




0.009




0.018




 




13.2




/




/




/




/




/




For welding 13%Cr stainless steels (e.g: SUS403、410).




KDC-YA430(Q)




E430T-1




YF430C




0.060




1.12




0.53




0.012




0.019




 




17.5




/




/




/




/




/




For welding 13%Cr ferritic stainless steel(e.g:SUS405、410L);and for the back weld when 13%Cr stainless steel is using in surfacing of carbon steel and low alloy steel.